professional factory provide SV-8890 Two-component Silicone Structural Glazing Sealant Supply to European

professional factory provide SV-8890 Two-component Silicone Structural Glazing Sealant Supply to European
  • professional factory provide SV-8890 Two-component Silicone Structural Glazing Sealant Supply to Europeanprofessional factory provide SV-8890 Two-component Silicone Structural Glazing Sealant Supply to European

Short Description:

Description SV8890 is neutral curing, designed for glass, stone, marble, granite, aluminum curtain wall and glass daylighting roof and metal structural engineering structural adhesive seal designed silicone sealant structure, excellent bonding performance of structure and the weathering resistance, after artificial accelerated weathering test, various physical and chemical properties have no obvious change in the sealant. When using, SV8890 with dedicated two-component glue machine constructi...


Product Detail

Attentions

Application

Product Tags

We will devote ourselves to providing our esteemed customers with the most enthusiastically thoughtful services for professional factory provide SV-8890 Two-component Silicone Structural Glazing Sealant Supply to European, We sincerely welcome all guests to set up business relationships with us on the basis of mutual benefits. Please contact us now. You will get our professional reply within 8 hours.


Description

SV8890 is neutral curing, designed for glass, stone, marble, granite, aluminum curtain wall and glass daylighting roof and metal structural engineering structural adhesive seal designed silicone sealant structure, excellent bonding performance of structure and the weathering resistance, after artificial accelerated weathering test, various physical and chemical properties have no obvious change in the sealant. When using, SV8890 with dedicated two-component glue machine construction, two kinds of components in accordance with the provisions, mixing ratio after curing form elastomer.

 

Key Features

1. None sag

2. Adjustable working time

3. Excellent adhesion to most building substrates

4. High bonding strength and modulus

5.12.5%movement capability

6. Silicone durability

 

Basic Application

1.Glass, stone, marble, granite, aluminum curtain wall and glass daylighting roof and metal structural engineering structural adhesive seal;

2.Insulating Glass of the second seal

3.Many other building and industrial applications

 

Technical data sheet

Test project Unit value
Flow, sagging or vertical flow mm 0
Operating time min 20
surface drying time(25℃,50%R.H.) min 40-60
Durometer Hardness Shore A 20-60
At 23 ℃ maximum tensile strength elongation % ≥100
Tensile strength(23℃) Mpa 0.9
Tensile strength(90℃) Mpa 0.68
Tensile strength(-30℃) Mpa 0.68
Tensile strength(flooding) Mpa 0.68
Tensile strength(flooding – ultraviolet) Mpa 0.68
Bond damage area % 5
Thermal aging(thermal weight loss) % ≤5
Thermal aging(crack)   No
 Thermal aging(efflorescence)   No

 

Certification

GB 16776

 

Color

Component A(Base) – White, Component B(Catalyst)- Black

 

Package

1. Component A(Base): (190L), Component B(Catalyst) (18.5L)

2. Component A(Base):24.5kg (18L), Component B(Catalyst): 1.9kg (1.8L)

 

Shelf life

12 months

 

Note

If you want the TDS or MSDS or other details, please contact with our sales person.

  • Previous:
  • Next:



  • This post cover Polyethylene Water Tank Repair – Crack. We show you how to repair a crack in a Polyethylene Water Tank, but the same method can be used for anything made of polyethylene, including canoes, kayaks, or anything else.
    The Tank
    I bought two 1550-gallon polyethylene tanks that I found on Craig’s list. I bought both for $450, which is about half of what one tank costs. Both tanks needed a little repair, but it was still a good deal. This post covers how to repair a crack. I’ll do another post in the future on how to repair a hole or gouge.
    The Crack
    The crack that I’m working on looks like it happened by an object hitting the tank and creating the crack with one half of the cracked piece knocked inward.
    Clean
    The first step was to clean the tank. I did this with a brush, water, and mild dish soap. I washed the outside of the tank just like I would a car. This prevents dirt and debris from getting into the repaired area. On the inside, the tank had some sand in it. I took my shop vac in and vacuumed up all of the dirt on the inside and wiped down the repair area with a wet rag.
    Level the Crack
    The next step is to level the crack. The two pieces on either side of the crack do not line up, so I stuck a screwdriver in the crack and pried the inner piece out to line up with the outer piece.
    The Welder
    They make a kit for welding polyethylene. I bought my kit from Amazon and it cost just over $100. I’ll include a link to that below. The welding kit is like a big hot soldering iron with sticks of polyethylene that you use to fill in gaps.



    Watch as a seasoned expert demonstrates how to install spline while repairing a sliding screen door in this free online video about home maintenance.

    Expert: Don Golden
    Bio: Don Golden has been in the business of buying and remodeling homes in the Los Angeles area for more than 15 years.
    Filmmaker: Louis Nathan

    Related Products

    WhatsApp Online Chat !