China Cheap price CV-709 silicone sealant for PV moudels Wholesale to Italy

China Cheap price CV-709 silicone sealant for PV moudels Wholesale to Italy
  • China Cheap price CV-709 silicone sealant for PV moudels Wholesale to ItalyChina Cheap price CV-709 silicone sealant for PV moudels Wholesale to Italy
  • China Cheap price CV-709 silicone sealant for PV moudels Wholesale to ItalyChina Cheap price CV-709 silicone sealant for PV moudels Wholesale to Italy
  • China Cheap price CV-709 silicone sealant for PV moudels Wholesale to ItalyChina Cheap price CV-709 silicone sealant for PV moudels Wholesale to Italy

Short Description:

Description CV709 is a high-performance silicone sealant, one-component oxime type room temperature curing silicone rubber, has excellent weather resistance, high thixotropy, after curing for solar components involved in the base material has good caking property, by TUV for environmental requirements of the ROHS, UL E339949   Key Features 1. 100% silicone 2. No sag 3. high thixotropy 4. Water & weatherproof 5. For solar components involved in the base material has good bonding   Basic Ap...


Product Detail

Attentions

Application

Product Tags

We will make every effort to be outstanding and perfect, and accelerate our steps for standing in the rank of international top-grade and high-tech enterprises for China Cheap price CV-709 silicone sealant for PV moudels Wholesale to Italy, We, with open arms, invite all interested buyers to visit our website or contact us directly for further information.


Description

CV709 is a high-performance silicone sealant, one-component oxime type room temperature curing silicone rubber, has excellent weather resistance, high thixotropy, after curing for solar components involved in the base material has good caking property, by TUV for environmental requirements of the ROHS, UL E339949

 

Key Features

1. 100% silicone

2. No sag

3. high thixotropy

4. Water & weatherproof

5. For solar components involved in the base material has good bonding

 

Basic Application

1.Solar module frame seal

2.The adhesive of the solar energy back to the terminal block

3.General industrial assembly with seal

 

Technical data sheet

Test standard Test project Unit value
Before curing——25℃,50%R.H.
  specific gravity g/ml 1.34-1.40
GB13477 Operating time min 15
GB13477 surface drying time(25℃,50%R.H.) min 40-60
3 days after curing——25℃,50%R.H.
  Temperature range -55~200
GB13477 Durometer Hardness Shore A 40~55
  The ultimate tensile strength Mpa ≥2
GB13477 Breaking elongation % 300-600
  Aluminum bonding shear strength Mpa ≥1.5
Electrical properties
  Breakdown voltage Kv/mm ≥20
  Volume resistance ohm.cm 9E+14
  Dielectric constant   3.1@50Hz

 

Certification

UL E339949; TUV

 

Color

Black, White

 

Package

300ml in cartridge * 24 per box, 500ml in sausage *20 per box

 

Shelf life

12 months

 

Note

If you want the TDS or MSDS or other details, please contact with our sales person.

  • Previous:
  • Next:



  • Huge thanks to our partners in crime;

    SIVE: https://www.youtube.com/user/IISIVEII
    BELLA + CANVAS: https://bit.ly/2t84DvI

    Ok guys, you asked for a screen print comparison so here it is. See how different ink types in screen printing come out!

    We have printed SIVE’s artwork onto 50/50 & 100% cotton garments, including plastisol, plastisol (puff), plastisol (softhand), we’ve also tested discharge inks & water based inks.

    If you are interested to understand the different types of screen printing methods and how they stack up, this is a great starting point.



    Terry talks about Tyvek which is a rain shield that protects the house from moisture. When water goes through a homes siding, it hypothetically hits this barrier and runs down to the ground. Terry further notes that the rain shield does not provide air sealing; instead, all the air sealing is already taking place behind the Tyvek in the polyisocyanurate foam, OSB, and behind the OSB where the spray foam has been applied.

    Furring strips are put over the Tyvek, so that when siding is placed over it, there is an air space between the siding and rain shield. In other words, air can circulate beneath the siding to dry it out if it gets too wet thus avoiding a possibility of deterioration. The window trim is then put up on top of the furring strips. A bug screen is then applied on top and bottom of the furring strips and Tyvek. The siding, fiber cement Hardie board, is finally put on. The practice of putting on furring strips on top of the rain shield is different from traditional building where this step is skipped; instead, the siding is put right on top of the rain shield.

    Related Products

    WhatsApp Online Chat !